Datasheet: Nitronic** 50
Nitronic 50 Exhibits corrosion resistance and that is superior to type 316 Stainless Steel. It has good mechanical properties at ambient and sub-zero temperatures. Unlike other austenitic stainless steels, it does not become magnetic when cold worked or cooled to sub-zero temperatures.
Nitronic 50 is also known as Aquamet 2, Aquamet 22, and Temet 25.
Available in all profile options
Superior corrosion resistance to type 316 stainless steel.
Good mechanical properties at ambient and sub-zero temperatures.
Does not become magnetic when cold worked or cooled to sub-zero temperatures.
Components in processing environments like:
– marine
– petroleum
– petrochemical
– fertilizer
– pulp and paper
W.Nr. 1.3964
UNS S20910
AWS 165
ISO 15156-3 (NACE MR0175)
Element | Min % | Max % |
---|---|---|
C | – | 0.06 |
Si | – | 1.00 |
Mn | 4.0 | 6.0 |
Ni | 11.5 | 13.5 |
Cr | 20.5 | 23.5 |
S | – | 0.03 |
P | – | 0.04 |
Mo | 1.5 | 3.0 |
N | 0.20 | 0.40 |
V | 0.10 | 0.30 |
Nb/Cb | 0.10 | 0.30 |
Fe | bal |
Density | Melting Point | Coefficient of Expansion | Modulus of Rigidity | Modulus of Elasticity |
---|---|---|---|---|
7.88 g/cm³ | 1415 – 1450 °C | 16.2 μm/m °C (20 – 100 °C) | 78.9 kN/mm² | 196.5 kN/mm² |
0.285 lb/in³ | 2579 – 2642 °F | 9.0 x 10-6 in/in °F (70 – 200 °F) | 11444 ksi | 28500 ksi |
Condition as supplied by AWI | Type | Temperature | Time | Cooling |
---|---|---|---|---|
Annealed or Spring Temper | Stress Relieve | 250 °C (480 °F) | 1 Hr | Air |
Solution Annealed | ||
---|---|---|
Approx. tensile strength | <1000 N/mm² | <145 ksi |
Approx. operating temperature | -200 to +300 °C | -330 to +570 °F |
Spring Temper | ||
---|---|---|
Approx. tensile strength | 1300 – 2200 N/mm² | 189 – 319 ksi |
Approx. operating temperature | -200 to +300 °C | -330 to +570 °F |
The above tensile strength ranges are typical. If you require different please ask.
*Trade name of AK Steel